IN738LC is an important Ni-based superalloy widely used to make hot section components in gas turbine engines. It has excellent high temperature mechanical properties combined with good processability.

This guide provides a detailed overview of IN738LC including its composition, properties, processing, applications, advantages, limitations, suppliers, and comparisons with alternative superalloys.

入門 IN738LC Superalloy

IN738LC is a precipitation hardenable Nickel-based superalloy with the following key characteristics:

  • 優れた高温強度と耐クリープ性
  • Good thermal fatigue and oxidation resistance
  • Retains properties up to ~1100°C
  • Composition optimized for processability
  • Versatile applications in gas turbines
  • Available as sheet, plate, bar and forged parts
  • Can be welded using suitable techniques

Its balanced properties make IN738LC suitable for a wide range of gas turbine components operating under demanding conditions.

in738lc

Chemical Composition of IN738LC

The nominal chemical composition of IN738LC is:

IN738LC Chemical Composition

エレメント重量 %
ニッケルバル
クロム16.0
コバルト8.5
アルミニウム3.4
チタン3.4
タンタル1.7
カーボン0.11
ボロン0.001
  • Nickel provides the matrix and improves ductility
  • Chromium for hot corrosion and oxidation resistance
  • Refractory elements like Ta, Ti, W for strengthening
  • Carbon/boron for grain boundary strengthening
  • Optimized composition for weldability

The balanced alloy design provides a combination of high temperature strength, ductility, and fabricability.

Physical and Mechanical Properties of IN738LC

物理的性質

  • Density: 8.19 g/cm3
  • Melting range: 1315-1370°C
  • Thermal conductivity: 11 W/m-K
  • Modulus of elasticity: 205 GPa
  • Electrical resistivity: 125 μΩ-cm

Mechanical Properties at Room Temperature

  • Tensile strength: 1035 MPa
  • 0.2% Yield strength: 965 MPa
  • Elongation: 22%
  • Fatigue strength: 590 MPa

High Temperature Mechanical Properties

  • Tensile strength:
    • 750 MPa at 704°C
    • 255 MPa at 982°C
  • Rupture strength:
    • 240 MPa at 760°C (100 hrs)
    • 170 MPa at 982°C (100 hrs)

The properties make it suitable for long term service upto ~9500C with appropriate design margins.

Key Applications of IN738LC Superalloy

IN738LC finds application in:

  • Gas turbine hot section parts:
    • 燃焼器ライナー
    • Transition ducts
    • Turbine nozzles
    • Stage 1 & 2 turbine blades and vanes
  • Rocket engine combustion chambers
  • Heat treatment fixtures
  • Nuclear fuel rods
  • Chemical process industry components

Its versatility makes it useful across several critical high temperature applications in demanding environments.

Manufacturing and Processing of IN738LC

Important manufacturing aspects for IN738LC include:

溶解

  • Vacuum induction melting and vacuum arc remelting
  • Ensures chemical homogeneity

Forming

  • Hot working above 1150°C
  • Cold working for sheet and foils

熱処理

  • Solution treatment – 1120°C, fast cooled
  • Precipitation hardening – 845°C, 24 hours, air cooled

接合

  • Electron beam and vacuum brazing
  • Fusion welding using matching filler alloys

コーティング

  • Diffusion aluminide and overlay coatings
  • Thermal barrier coatings

Control of melting, hot working, heat treatment, joining and coatings is critical to achieve optimal properties.

Why Choose IN738LC Superalloy?

Some key advantages of IN738LC:

  • 優れた高温機械特性
  • Retains strength and creep resistance upto ~1100°C
  • Good thermal fatigue and oxidation resistance
  • Better processing flexibility versus other Ni-superalloys
  • Can be fused welded for fabricating complex parts
  • Available as sheet, plate, bar and forgings
  • Cost-effective compared to contemporary alloys
  • Established processing methods and data available
  • Approved for critical engine components

The balanced properties and processability of IN738LC make it an ideal choice for many gas turbine hot section components.

Limitations of Using IN738LC Superalloy

Some limitations to consider while using IN738LC are:

  • Lower high temperature strength than latest single crystal alloys
  • Not suitable for very high temperature turbine parts
  • Susceptible to strain-age cracking during forming
  • Requires carefully controlled heat treatment
  • Lower oxidation resistance than Nb-bearing alloys
  • Weldability not as good as IN718
  • Forming can induce residual stresses

IN738LC may not be suitable for very demanding environments. Proper design and processing is key to mitigate limitations.

IN738LC Superalloy Suppliers

Some leading suppliers of IN738LC alloys include:

  • Special Metals Corporation
  • Allegheny Technologies
  • ヘインズ・インターナショナル
  • カーペンター・テクノロジー
  • サンドビック・マテリアル・テクノロジー
  • Precision Castparts Corp.

IN738LC is available as:

  • Sheet / Plate
  • Bar
  • Forging stock
  • Wire
  • 溶接消耗品

Various product forms are offered to suit different fabrication requirements.

IN738LC Superalloy Costs

IN738LC Cost Indicators

  • Sheet: $90-110/kg
  • Bar: $100-120/kg
  • Forging stock: $110-130/kg
  • Costs depend on size, quantity, supplier, and raw material costs
  • Generally 10-15% economical than contemporary Ni-alloys
  • Requires high purity raw materials increasing costs

IN738LC provides cost-effective performance for many gas turbine applications. Long term agreements can secure stable pricing.

Comparison of IN738LC with Alternative Superalloys

Comparison with IN718

  • IN738LC has higher temperature capability
  • Better creep and thermal fatigue properties
  • Reduced forming issues versus IN718
  • IN718 offers better weldability

Comparison with IN713C

  • IN738LC has higher tensile and creep strength
  • Improved phase stability
  • Lower expansion coefficient than IN713C
  • IN713C offers better fabricability

Comparison with Contemporary Ni-Alloys

  • Advanced alloys like Renes N5, CMSX-4 offer higher temperature strength
  • However, they also have poorer fabricability and higher costs
  • IN738LC provides a cost-effective combination of properties
in738lc

よくあるご質問

Q: What are the main applications of IN738LC alloy?

A: Main applications are gas turbine hot section parts like combustors, transition ducts, nozzles, turbine vanes and blades. It is also used in rocket engines and nuclear fuel rods.

Q: What are the key properties of IN738LC?

A: It has excellent high temperature mechanical properties upto 1100°C, good fatigue and oxidation resistance, high strength, and better fabricability than other Ni-superalloys.

Q: What heat treatment is used for IN738LC?

A: Solution treatment at 1120°C followed by precipitation hardening at 845°C/24 hrs. Controlled heat treatment is critical to achieve required properties.

Q: How is IN738LC welded?

A: Electron beam and vacuum brazing are commonly employed. Fusion welding can also be done using matching filler alloys and carefully controlled processes.

Q: What are the alternatives to IN738LC?

A: Alternatives include IN718, IN713C and advanced Ni-alloys like Renes N5, CMSX. Each has relative pros and cons versus IN738LC.

Q: Does IN738LC need coatings?

A: Diffusion aluminide or overlay coatings may be used. Thermal barrier coatings are beneficial for turbine components. Coatings enhance oxidation and corrosion resistance.

Q: What precautions are needed when machining IN738LC?

A: It requires high cutting speeds with sharp tooling to avoid work hardening effects. Generous coolant is essential. Machining can induce residual stresses needing relief heat treatment.

Q: Where is IN738LC used in gas turbine engines?

A: It is widely used for combustion liners, transition ducts, nozzles, stage 1 and 2 turbine vanes and blades in the hot sections.

Q: What forms is IN738LC available in?

A: Common product forms include sheet, plate, bar, forgings, wire. Various forms are used to fabricate hot section components based on requirements.

より多くの3Dプリントプロセスを知る

シェアする

フェイスブック
ツイッター
LinkedIn
WhatsApp
電子メール
メタル3dpロゴ小

Metal3DP Technology Co., LTDは、中国青島に本社を置く積層造形ソリューションのリーディングプロバイダです。当社は、3Dプリンティング装置と産業用途の高性能金属粉末を専門としています。

お問い合わせは、最良の価格とあなたのビジネスのためのカスタマイズされたソリューションを取得します!

関連記事

炭化チタン粉

炭化チタン粉末

炭化チタン粉末は、高い硬度、耐摩耗性、熱伝導性、および耐熱性を必要とする様々な産業用途に使用される非常に硬いセラミック材料です。

続きを読む
純ニッケル粉

純ニッケル粉

純ニッケル粉末は、ユニークな特性を持つ汎用性の高い金属粉末であり、様々な産業分野の高度な用途に適しています。この記事では

続きを読む

Met3DPについて

ビデオ再生

最新情報

製品

お問い合わせ

ご質問は?今すぐメッセージをお送りください!私たちはあなたのメッセージを受け取った後、チーム全体であなたの要求を提供します。 

メタル3DPの
製品パンフレット

最新のテクノロジー、イノベーション、企業ニュースをお届けします。